The relative reactivities of pulverized samples (100–200 mesh) of 3 marcasite and 7 pyrite specimens from various sources were determined at 25°C and pH 2.0 in ferric chloride solutions with initial ferric iron concentrations of 10?3 molal. The rate of the reaction:
FeS2 + 14Fe3+ + 8H2O = 15Fe2+ + 2SO2?4 + 16H+
was determined by calculating the rate of reduction of aqueous ferric ion from measured oxidation-reduction potentials. The reaction follows the rate law:
?dmFe3+dt = k(AM)mFe3+
where mFe3+ is the molal concentration of uncomplexed ferric iron, k is the rate constant and AM is the surface area of reacting solid to mass of solution ratio. The measured rate constants, k, range from 1.0 × 10?4 to 2.7 × 10?4 sec?1 ± 5%, with lower-temperature/early diagenetic pyrite having the smallest rate constants, marcasite intermediate, and pyrite of higher-temperature hydrothermal and metamorphic origin having the greatest rate constants. Geologically, these small relative differences between the rate constants are not significant, so the fundamental reactivities of marcasite and pyrite are not appreciably different.The activation energy of the reaction for a hydrothermal pyrite in the temperature interval of 25 to 50°C is 92 kJ mol?1. This relatively high activation energy indicates that a surface reaction controls the rate over this temperature range. The BET-measured specific surface area for lower-temperature/early diagenetic pyrite is an order of magnitude greater than that for pyrite of higher-temperature origin. Consequently, since the lower-temperature types have a much greater AM ratio, they appear to be more reactive per unit mass than the higher temperature types.  相似文献   

2.
Solubility curves were determined for a synthetic gibbsite and a natural gibbsite (Minas Gerais, Brazil) from pH 4 to 9, in 0.2% gibbsite suspensions in 0.01 M NaNO3 that were buffered by low concentrations of non-complexing buffer agents. Equilibrium solubility was approached from oversaturation (in suspensions spiked with Al(NO3)3 solution), and also from undersaturation in some synthetic gibbsite suspensions. Mononuclear Al ion concentrations and pH values were periodically determined. Within 1 month or less, data from over-and undersaturated suspensions of synthetic gibbsite converged to describe an equilibrium solubility curve. A downward shift of the solubility curve, beginning at pH 6.7, indicates that a phase more stable than gibbsite controls Al solubility in alkaline systems. Extrapolation of the initial portion of the high-pH side of the synthetic gibbsite solubility curve provides the first unified equilibrium experimental model of Al ion speciation in waters from pH 4 to 9.The significant mononuclear ion species at equilibrium with gibbsite are Al3+, AlOH2+, Al(OH)+2 and Al(OH)?4, and their ion activity products are 1K50 = 1.29 × 108, 1Ks1 = 1.33 × 103, 1Ks2 = 9.49 × 10?3 and 1Ks4 = 8.94 × 10?15. The calculated standard Gibbs free energies of formation (ΔG°f) for the synthetic gibbsite and the A1OH2+, Al(OH)+2 and Al(OH)?4 ions are ?276.0, ?166.9, ?216.5 and ?313.5 kcal mol?1, respectively. These ΔG°f values are based on the recently revised ΔG°f value for Al3+ (?117.0 ± 0.3 kcal mol?1) and carry the same uncertainty. The ΔG°f of the natural gibbsite is ?275.1 ± 0.4 kcal mol?, which suggests that a range of ΔG°f values can exist even for relatively simple natural minerals.  相似文献   

3.
4.
Cyclic voltammetry has been done for Ni2+, Co2+, and Zn2+ in melts of diopside composition in the temperature range 1425 to 1575°C. Voltammetric curves for all three ions excellently match theoretical curves for uncomplicated, reversible charge transfer at the Pt electrode. This implies that the neutral metal atoms remain dissolved in the melt. The reference electrode is a form of oxygen electrode. Relative to that reference assigned a reduction potential of 0.00 volt, the values of standard reduction potential for the ions are E1 (Ni2+Ni0, diopside, 1500°C) = ?0.32 ± .01 V, E1 (Co2+Co0, diopside, 1500°C) = ?0.45 ± .02 V, and E1 (Zn2+Zn0, diopside, 1500°C) = ?0.53 ± .01 V. The electrode reactions are rapid, with first order rate constants of the order of 10?2 cm/sec. Diffusion coefficients were found to be 2.6 × 10?6 cm2/sec for Ni2+, 3.4 × 10?6 cm2/sec for Co2+, and 3.8 × 10?6 cm2/sec for Zn2+ at 1500°C. The value of E1 (Ni2+Ni0, diopside) is a linear function of temperature over the range studied, with values of ?0.35 V at 1425°C and ?0.29 V at 1575°C. At constant temperature the value of E1 (Ni2+Ni0, 1525°C) was not observed to vary with composition over the range CaO · MgO · 2SiO2 to CaO·MgO·3SiO2 or from 1.67 CaO·0.33MgO·2SiO2 to 0.5 CaO·1.5MgO·2SiO2. The value for the diffusion coefficient for Ni2+ decreased by an order of magnitude at 1525°C over the compositional range CaO · MgO · 1.25SiO2 to CaO · MgO · 3SiO2. This is consistent with a mechanism by which Ni2+ ions diffuse by moving from one octahedral coordination site to another in the melt, with the same Ni2+ species discharging at the cathode regardless of the SiO2 concentration in the melt.  相似文献   

5.
The synthetic chelating agent ethylenediaminetetraacetic acid (EDTA) has been used to evaluate the stoichiometric solubility product of galena (PbS) at 298°K: Ks2 = aPb2+aHS?aH+ This method circumvents the possible uncertainties in the stoichiometry and stability of lead sulfide complexes. At infinite dilution, Log Ks2 = ?12.25 ±0.17, and at an ionic strength corresponding to seawater (I = 0.7 M), Log Ks2 = ?11.73 ± 0.05. Using the value of Ks2 at infinite dilution, and the free energies of formation of HS? and Pb2+ at 298°K (literature values), the free energy of formation of PbS at 298°K is computed to be ?79.1 ± 0.8 KJ/mol (?18.9 Kcal/mol). Galena is shown to be more than two orders of magnitude more soluble than indicated by calculations based on previous thermodynamic data.  相似文献   

6.
Solution calorimetric measurements compared with solubility determinations from the literature for the same samples of gibbsite have provided a direct thermochemical cycle through which the Gibbs free energy of formation of [Al(OH)4 aq?] can be determined. The Gibbs free energy of formation of [Al(OH)4 aq?] at 298.15 K is ?1305 ± 1 kJ/mol. These heat-of-solution results show no significant difference in the thermodynamic properties of gibbsite particles in the range from 50 to 0.05 μm.The Gibbs free energies of formation at 298.15 K and 1 bar pressure of diaspore, boehmite and bayerite are ?9210 ± 5.0, ?918.4 ± 2.1 and ?1153 ± 2 kJ/mol based upon the Gibbs free energy of [A1(OH)4 aq?] calculated in this paper and the acceptance of ?1582.2 ± 1.3 and ?1154.9 ± 1.2 kJ/mol for the Gibbs free energy of formation of corundum and gibbsite, respectively.Values for the Gibbs free energy formation of [Al(OH)2 aq+] and [AlO2 aq?] were also calculated as ?914.2 ± 2.1 and ?830.9 ± 2.1 kJ/mol, respectively. The use of [AlC2 aq?] as a chemical species is discouraged.A revised Gibbs free energy of formation for [H4SiO4aq0] was recalculated from calorimetric data yielding a value of ?1307.5 ± 1.7 kJ/mol which is in good agreement with the results obtained from several solubility studies.Smoothed values for the thermodynamic functions CP0, (HT0 - H2980)T, (GT0 - H2980)T, ST0 - S00, ΔH?,2980 kaolinite are listed at integral temperatures between 298.15 and 800 K. The heat capacity of kaolinite at temperatures between 250 and 800 K may be calculated from the following equation: CP0 = 1430.26 ? 0.78850 T + 3.0340 × 10?4T2 ?1.85158 × 10?4T212 + 8.3341 × 106 T?2.The thermodynamic properties of most of the geologically important Al-bearing phases have been referenced to the same reference state for Al, namely gibbsite.  相似文献   

7.
The carbonato and hydrogencarbonato complexes of Mg2+ were investigated at 25 and 50° in solutions of the constant ClO4? molality (3 M) consisting preponderantly of NaClO4. The experimental data could be explained assuming the following equilibria: Mg2+ + CO2B + H2O ag MgHCO+3 + H+, log 1β1 = ?7.644 ± 0.017 (25°), ?7.462 ± 0.01 1 (50°), Mg2+ + 2 CO2g + 2 H2Oag Mg(HCO3)02 ± 2 H+, log 1β2 = ?15.00 ± 0.14 (25°), ?15.37 ± 0.39 (50°), Mg2+ + CO2g + H2Oag MgCO03 + 2 H+, log 1k1 = ?15.64 ± 0.06 (25°),?15.23 ± 0.02 (50°), with the assumption γMgCO30 = γMg(HCO3)02, ΔG0(I = 0) for the reaction MgCO03 + CO2g + H2O = Mg(HCO3)02 was estimated to be ?3.91 ± 0.86 and 0.6 ± 2.4 kJ/mol at 25 and 50°C, respectively. The abundance of carbonate linked Mg(II) species in fresh water systems is discussed.  相似文献   

8.
Measurement of solubility as a function of pressure allows calculation of 3V?1. Using this experimental approach, the best estimate of 3V?1 for the dissolution of aged amorphous silica in salt water or seawater at 0–2°C is ?9.9 cm3 mol?1 (standard error = 0.4 cm3 mol?1). This gives V?Si(OH)4(aq)= 55 ± 5 cm3mol?1, which compares well with other published values of V?Si(OH)4(aq).  相似文献   

9.
The spectrophotometric measurements of chloro complexes of lead in aqueous HCl, NaCl, MgCl2 and CaCl2 solutions at 25°C have been analyzed using Pitzer's specific interaction equations. Parameters for activity coefficients of the complexes PbCl+, PbCl20 and PbCl3? have been determined for the various media. Values of K1 = 30.0 ± 0.6, K2 = 106.7 ± 2.1 and K3 = 73.0 ± 1.5 were obtained for the cumulative formation constants. [Pb2+ + nCl? → PbCln2?n)]. These values are in reasonable agreement with literature data. The Pitzer parameters for the PbCl ion pairs in various media were used to calculate the speciation of Pb2+ in an artificial seawater solution.  相似文献   

10.
A linear correlation exists between the standard Gibbs free energies of formation of calcite-type carbonates (MCO3) and the corresponding conventional standard Gibbs free energies of formation of the aqueous divalent cations (M2+) at 25 °C and 1 bar ΔGMCO30 = m(ΔGf,M2+0) ? 141,200 cal · mole?1 where m is equal to 0.9715. This relationship enables prediction of the standard free energies of formation of numerous hypothetical carbonates with the calcite structure. Associated uncertainties typically range from about ± 250 to 600 cal · mole?1. An important consequence of the above correlation is that the thermodynamic equilibrium constant for the distribution of two trace elements M and N between carbonate mineral and aqueous solution at 25 °C and 1 bar is proportional to the free energy difference between the corresponding two aqueous ions: In KM-N = m ? 1298.15RG?f,M2+0 ? ΔG?f,N2+0)Combination of predicted standard free energies, entropies and volumes of carbonate minerals at 25°C and 1 bar with standard free energies of aqueous ions and the equation of state in Helgesonet al. (1981) enables prediction of the thermodynamic equilibrium constant for trace element distribution between carbonates and aqueous solutions at elevated temperatures and pressures. Interpretation of the thermodynamic equilibrium constant in terms of concentration ratios in the aqueous phase is considerably simplified if pairs of divalent trace elements are considered that have very similar ionic radii (e.g., Sr2+Pb2+, Mg2+Zn2+). In combination with data for the stabilities of complex ions in aqueous solutions, the above calculations enable useful limits to be placed on the concentrations of trace elements in hydrothermal solutions.  相似文献   

11.
Equations are developed for calculating the density of aluminosilicate liquids as a function of composition and temperature. The mean molar volume at reference temperature Tr, is given by Vr = ∑XiV?oi + XAV?oA, where the summation is taken over all oxide components except A12O3, X stands for mole fraction, V?oi terms are constants derived independently from an analysis of volume-composition relations in alumina-free silicate liquids, and V?oA is the composition-dependent apparent partial molar volume of Al2O3. The thermal expansion coefficient of aluminosilicate liquids is given by α = ∑Xi\?gaio + XA\?gaAo, where \?gaio terms are constants independent of temperature and composition, and \?gaoA is a composition-dependent term representing the effect of Al2O3 on the thermal expansion. Parameters necessary to calculate the volume of silicate liquids at any temperature T according to V(T) = Vrexp[α(T-Tr)], where Tr = 1400°C have been evaluated by least-square analysis of selected density measurements in aluminosilicate melts. Mean molar volumes of aluminosilicate liquids calculated according to the model equation conform to experimentally measured volumes with a root mean square difference of 0.28 ccmole and an average absolute difference of 0.90% for 248 experimental observations. The compositional dependence of V?oA is discussed in terms of several possible interpretations of the structural role of Al3+ in aluminosilicate melts.  相似文献   

12.
Potentiometric measurements in dilute sodium borate solutions with added alkali earth chlordie salts yield the following expressions for the dissociation constants of alkali earth borate ion pairs from 10 to 50°C:
pK(MgH2BO3+=1.266+0.001204 T
pK(CaH2BO3+=1.154+0.002170 T
pK(SrH2BO3+=1.033+0.001738 T
pK(BaH2BO3+=1.942+0.001850 T
where T is in °K. Enthalpies for the dissociation reactions at 25°C are less than 1 kcal./mole for all the alkali earth borate ion pairs.Values for pK(NaH2BO3°) from 5 to 55°C computed from the experimental data of Owen and King are in good agreement with those determined potentiometrically. The average value from both methods is 0.22 ± 0.1 at 25°C.Application to seawater of computed pK's for MgH2BO3+, CaH2BO3+ and NaH2BO30 yields an apparent dissociation constant for boric acid of 8.73 vs. 8.70 measured by Lyman, 8.68 by Buch and 8.73 by Byrne and Kester.  相似文献   

13.
Stability constants of hydroxocomplexes of Al(III):Al(OH)2+ and A1(OH)4? have been measured in the 20–70°C temperature range by reactions involving only dissolved species. The stability constant 1K1 of the first complex ion is studied by measuring pH of solutions of aluminium salts at several concentrations. 1β4 of aluminate ion is deduced from equilibrium constants of the reaction between the trioxalato aluminium (III) complex ion and Al3+ in acid medium, and between the same complex ion and A1(OH)4? in alkaline medium. The K values and the associated ΔH are 1K1 = 10?5.00 and ΔH1 = 11.8 Kcal; 1β4 = 10?22.20 and ΔH4 = 42.45 Kcal. These last results are not in agreement with the values of recent tables for ΔG0? and ΔH0? of Al3+ and Al(OH)4?. We suggest a consistent set of data for dissolved and solid Al species and for some aluminosilicates.  相似文献   

14.
40Ar39Ar age spectrum analyses of three microcline separates from the Separation Point Batholith, northwest Nelson, New Zealand, which cooled slowly (~5°C-Ma?1) through the temperature zone of partial radiogenic 40Ar accumulation are characterized by a linear age increase over the first 65 percent of gas release with the lowest ages (~80 Ma) corresponding to the time that the samples cooled below about 100°C. The last 35 percent of 39Ar released from the microclines yields plateau ages (103,99 and 93 Ma) which reflect the different bulk mineral ages, and correspond to cooling temperatures between about 130 to 160°C. Theoretical calculations confirm the likelihood of diffusion gradients in feldspars cooling at rates ≤5°C-Ma?1. Diffusion parameters calculated from the 39Ar release yield an activation energy, E = 28.8 ± 1.9 kcal-mol?1, and a frequency factor/grain size parameter, D0l2 = 5.6?3.9+14sec?1. This Arrhenius relationship corresponds to a closure temperature of 132 ± 13°C which is very similar to the independently estimated temperature. From the observed diffusion compensation correlation, this D0l2 implies an average diffusion half-width of about 3 μm, similar to the half-width of the perthite lamellae in the feldspars. The range in microcline K-Ar ages from the Separation Point Batholith is the result of relatively small temperature differences within the pluton during cooling. Comparison of the diffusion laws determined for microcline with those for anorthoclases and other homogeneous K-feldspars (E = 40 to 52 kcal-mol?1) reveals that Ar diffusion is more highly temperature dependent in the disordered structural state than in the ordered structural state. Previously published U-shaped age spectra are probably the result of the superimposition of excess 40Ar upon diffusion profiles of the kind described here.  相似文献   

15.
Chemical equilibrium between sodium-aluminum silicate minerals and chloride bearing fluid has been experimentally determined in the range 500–700°C at 1 kbar, using rapid-quench hydrothermal methods and two modifications of the Ag + AgCl acid buffer technique. The temperature dependence of the thermodynamic equilibrium constant (K) for the reaction NaAlSi3O8 + HClo = NaClo + 12Al2SiO5, + 52SiO2 + 12H2O Albite Andalusite Qtz. K = (aNaClo)(aH2O)1/2(aHClo) can be described by the following equation: log k = ?4.437 + 5205.6/T(K) The data from this study are consistent with experimental results reported by Montoya and Hemley (1975) for lower temperature equilibria defined by the assemblages albite + paragonite + quartz + fluid and paragonite + andalusite + quartz + fluid. Values of the equilibrium constants for the above reactions were used to estimate the difference in Gibbs free energy of formation between NaClo and HClo in the range 400–700°C and 1–2 kbar. Similar calculations using data from phase equilibrium studies reported in the literature were made to determine the difference in Gibbs free energy of formation between KClo and HClo. These data permit modelling of the chemical interaction between muscovite + kspar + paragonite + albite + quartz assemblages and chloride-bearing hydrothermal fluids.  相似文献   

16.
The effect of presure on the solubility of minerals in water and seawater can be estimated from In
(KPspK0sp) + (?ΔVP + 0.5ΔKP2)RT
where the volume (ΔV) and compressibility (ΔK) changes at atmospheric pressure (P = 0) are given by
ΔV = V?(M+, X?) ? V?[MX(s)]ΔK = K?(M+, X?) ? K?[MX(s)]
Values of the partial molal volume (V?) and compressibilty (K?) in water and seawater have been tabulated for some ions from 0 to 50°C. The compressibility change is quite large (~10 × 10?3 cm3 bar?1 mol?1) for the solubility of most minerals. This large compressibility change accounts for the large differences observed between values of ΔV obtained from linear plots of In Ksp versus P and molal volume data (Macdonald and North, 1974; North, 1974). Calculated values of KPspKosp for the solubility of CaCO3, SrSO4 and CaF2 in water were found to be in good agreement with direct measurements (Macdonald and North, 1974). Similar calculations for the solubility of minerals in seawater are also in good agreement with direct measurements (Ingle, 1975) providing that the surface of the solid phase is not appreciably altered.  相似文献   

17.
Natural malachite is a well defined solid demonstrating reproducible solubility behavior over a wide range of pH. The following equilibrium constants associated with the malachite dissolution equilibrium at 25°C, 1 atm were determined:
Ksp = a2cu2+aCO32?K2wa2H+ = 3.5 ± 0.6 × 10?34
(infinite dilution)
K1sp = [Cu2+]2[CO2?3]K2wa2H+ = 10. ± 0.2 × 10?32
(0.72 ionic strength)
K′sp = m2Cu2+mCOsu2?3K2wa2H+ = 1.3 ± 0.1 × 10?28
(36.9‰ salinity seawater). The temperature dependence of a “mixed” equilibrium constant, Ksp+, of the form:
K2sp = [Cu2+]2mCO2?3K2wa2H+
has been measured at I = 0.72, yielding the relationship:
log K2sp = (? 9.8 ± 0.03) × 104(1T°K) + (1.52 ± 0.09)
within a 5–25°C temperature range. The effect of pressure on the solubility of malachite in water and seawater was estimated from partial molar volume and compressibility data. For 25 °C at infinite dilution K'sp (1000 bar)K'sp(0) = 240 and in seawater K′sp(1000)K'sp(0) = 44.Comparison of stoichiometric and apparent malachite equilibrium constants has been used to estimate the extent of copper(II) ion interaction at the ionic strength of seawater. In dilute carbonate medium (total alkalinity, TA = 2.4 meq/kg H2O, pH 8.3), 2.9% of total dissolved copper exists as the free copper(II) ion and in seawater (S = 36.9%., TA = 2.3 meq/kg H2O, pH = 8.1), [Cu2+]T(Cu) is 3.1%.Total dissolved copper levels of approximately 450–750 nMol/Kg are necessary to attain malachite saturation conditions in the open ocean. Observations of malachite particles suspended in seawater must be explained by precipitation or solid phase substitution reactions from localized environments rather than by direct precipitation from bulk seawater.  相似文献   

18.
Oxygen isotope exchange between BaSO4 and H2O from 110 to 350°C was studied using 1 m H2SO4-1 m NaCl and 1 m NaCl solutions to recrystallize the barite. The slow exchange rate (only 7% exchange after 1 yr at 110°C and 91% exchange after 22 days at 350°C in 1 m NaCl solution) prompted the use of the partial equilibrium technique. However, runs at 300 and 350°C were checked by complete exchange experiments. The temperature calibration curve for the isotope exchange is calculated giving most weight to the high temperature runs where the partial equilibrium technique can be tested. Oxygen isotope fractionation factors (α) in 1 m NaCl solution (110–350°C), assuming a value of 1.0407 for αCO2H2O at 25°C, are:
1031nαBaSO4?1 m NaCl = 2.64 (106T2) ? 5.3 ± 0.3
.These data, when corrected for ion hydration effects in solution (Truesdell, 1974), give the fractionation factors in pure water:
1031nαBaSO4H2O = 3.01 (106/T2) ?7.3 ± 0.1
.In the 1 m H2SO4-1 m NaCl runs, sulfur isotope fractionation between HSO?4 and BaSO4 is less than the detection limit of 0.4%. A barite-sulfide geothermometer is obtained by combining HSO?4H2S and sulfide-H2S calibration data.Barite in the Derbyshire ore field, U.K., appears to have precipitated in isotopic equilibrium with water and sulfur in the ore fluid at temperatures less than 150°C. At the Tui Mine, New Zealand, the barite-water geothermometer indicates temperatures of late stage mineralization in the range 100–200°C. A temperature of 350 ± 20°C is obtained from the barite-pyrite geothermometer at the Yauricocha copper deposit, Peru, and oxygen isotope analyses of the barite are consistent with a magmatic origin for the ore fluids.  相似文献   

19.
20.
The decay constant 87Rb has been redetermined by measuring the amount of radiogenic 87Sr produced over a period of 19 years, in 20 g samples of purified RbClO4, using isotope dilution techniques. The rubidium sample was spiked with 84Sr and the nanogram quantities of strontium separated by coprecipitation with Ba(NO3)2. Analyses were carried out on a 25cm, 90° sector mass spectrometer equipped with a Spiraltron electron multiplier. Measurement of three independent ratios permitted continuous monitoring of the ion beam fractionation. The average of nine determinations gives a value for the decay constant of 1.419(±0.012) × 10?11 yr?1 (2σ). [τ12 = 4.89(±0.04) × 1010yr.]  相似文献   