摘    要:考虑酸浓度和养护时间的影响,通过室内试验对比研究了酸污染红土的颗粒组成、比重和界限含水率等物理特性。研究结果表明:不洗盐、加分散剂,酸浓度较低时粉粒含量减小,酸浓度较高时粉粒含量增大;随养护时间延长,浓度较低时粉粒含量减小,浓度较高时粉粒含量先增后减;洗盐后粉粒含量减小,不加分散剂粉粒含量增大。酸污染红土的比重、液塑限与塑性指数随酸浓度的增大和养护时间的延长总体都呈减小的趋势。酸污染红土物理性质的变化可以从酸污染红土所存在的腐蚀、成盐和溶解三个阶段来解释。


关 键 词:酸污染红土  颗粒组成特性  比重特性  液塑限特性  腐蚀过程

Variation characteristics of physical properties of acid pollution laterite
BO Tong-zhen , HUANG Ying , SHI Chong-xi , WANG Ying , FENG Huan.Variation characteristics of physical properties of acid pollution laterite[J].Hydrogeology and Engineering Geology,2012,39(2):111-115.
Authors:BO Tong-zhen  HUANG Ying  SHI Chong-xi  WANG Ying  FENG Huan
Affiliation:(1. Kunming University of Science and Technology, Kunming, Yunnan 650051, China; 2. Yunnan College of Business Management, Kunming, Yunnan 650051, China)
Abstract:In this paper,a contrast study is made of the physical characteristics of acid pollution laterite by laboratory tests,including grain composition,specific gravity and boundaries moisture content,considering the influence of dispersing agent and salt-leaching.The results show that without dispersing agent and salt-leaching,the silt content decreases with lower acid concentration but increases with higher acid concentration.With the extended curing time,the silt content decreases with lower acid concentration,but decreases,then increases with higher acid concentration.Silt content decreases after salt-leaching,but increases without dispersing agent.The specific gravity,liquid limit and plastic limit,plasticity index of acid pollution laterite decrease with accrescent acid concentration and extended curing time.The changes in physical characteristics of acid pollution laterite are the combined result of corrosion stage,salt-forming stage and dissolution stage.
Keywords:acid pollution laterite  grain composition  specific gravity  liquid limit and plastic limit  corrosion process
本文献已被 CNKI 万方数据 等数据库收录!
点击此处可从《水文地质工程地质》浏览原始摘要信息
点击此处可从《水文地质工程地质》下载全文
设为首页 | 免责声明 | 关于勤云 | 加入收藏

Copyright©北京勤云科技发展有限公司    京ICP备09084417号-23

京公网安备 11010802026262号